N
Nibbles75
Before Christmas i tiled a bathroom floor in bisazza 10mmx10mmglass mosaics(paper fronted), black epoxy and theyve (WORD REMOVED) lifted.... The screed was anhydrite which iam aware of, so it was primed with benferprim, 2 coats and white flexi adhesive was used. Two other bathrooms and large kitchen floor have been tiled and nothing else has lifted. Only some grout cracking in the kitchen.
The property is a new build with approx 200m2 wet underfloor heating system. This had been on full blast soon after floor was tiled when we had the sub zero conditions in December. It was like working in the bahamas some days!
I personally think this is the main reason for the problem but im interested to see what other suggestions you guys may have to the cause of the problem??
The property is a new build with approx 200m2 wet underfloor heating system. This had been on full blast soon after floor was tiled when we had the sub zero conditions in December. It was like working in the bahamas some days!
I personally think this is the main reason for the problem but im interested to see what other suggestions you guys may have to the cause of the problem??
Last edited by a moderator: