F
fergal
We completed a contract about 6 months ago , in which part of the job had a number of GYVLON calcium sulphate floor screeds, now the main contractor has called us back on site because a number of the vinal flooring coverings had started to lift, To make a long story short the screed floor guys have been very fair ,the sanded the floor to remove laitace and recomanded a number of primers,which were passed on to the floor coverings contractor, we have also used the screed guys on two other jobs with out any problems. My question is has any body had any issues when using F BALL STOPGAP121 one coat system on GYVLON screeds, our floor covering contractor who used it, is now claiming that the issue is with moisture in the screed and the F BALL rep is claiming the same. I have done some homework on these screeds and even the screed contractor who layed it claims that all Acrylic primers should be dome with a two coat system 1 to 1 then neat.
Is this correct? I am also dissapointed in the F BALL rep as he seems to want to blame every thing other than his primier, but I found on the F BALL web site a data sheet for the STOPGAP121 and it says its a one coat system Acrylic and everyone else claims that for a proper job it should be two coats...............does any one know which is correct..???:mad2:
Is this correct? I am also dissapointed in the F BALL rep as he seems to want to blame every thing other than his primier, but I found on the F BALL web site a data sheet for the STOPGAP121 and it says its a one coat system Acrylic and everyone else claims that for a proper job it should be two coats...............does any one know which is correct..???:mad2: