lesterwilde
Hi folks, Have had 600 x600 porcelain tiles laid onto well cured ecternal screed slab.
Tiles where sold as exterior grade. The have a rough texture to them.
screed slab had been down six months.
Slab had Ardex exterior leveling compound on top of slab before tiling. Ardex exterior adhesive and grouts have been used for laying tiles. Tiles have been laid about 2 weeks.
Tiles had some soil staining on surface had to be washed down with jet wash.
The problem is white staining has appeared in big areas over tiles. Is this the dreaded effervescence salts coming through.
Any suugestions on what can be done to sort this problem out would very much apprecaited.
Thanks Lester
Tiles where sold as exterior grade. The have a rough texture to them.
screed slab had been down six months.
Slab had Ardex exterior leveling compound on top of slab before tiling. Ardex exterior adhesive and grouts have been used for laying tiles. Tiles have been laid about 2 weeks.
Tiles had some soil staining on surface had to be washed down with jet wash.
The problem is white staining has appeared in big areas over tiles. Is this the dreaded effervescence salts coming through.
Any suugestions on what can be done to sort this problem out would very much apprecaited.
Thanks Lester